Microwave-assisted low-oxygen roasting–weak magnetic separation for desulfurization and iron enrichment from refractory high-sulfur iron tailings: A theoretical feasibility-domain analysis

Jigang Zhao 1, Enlei Wang 1

1School of Mining Engineering, University of Science and Technology Liaoning, Liaoning, China

Abstract

Refractory high-sulfur iron tailings are difficult to upgrade because desulfurization and magnetic enrichment require opposing oxygen environments. Oxidizing roasting removes sulfur as gaseous oxides but produces weakly magnetic hematite rather than magnetite. This strictly theoretical study, without experimental validation, redefines this incompatibility as a search for a common operating mode. Using measured Anshan tailings as the compositional matrix and a constructed high-sulfur condition as the reactive scenario, coupled thermodynamic, kinetic and mass-balance calculations define the temperature–oxygen-pressure window, bound magnetite conversion and iron recovery, and characterize the trade-off between desulfurization and magnetite yield. Desulfurization and magnetization occur within a narrow low-oxygen window, where pyrite-derived sulfur acts as an internal reductant converting hematite to magnetite, while microwave selective heating preferentially energizes reactive phases. The feasible band contracts sharply with increasing temperature. Magnetite-associated iron reaches 31.38 g per 100 g of feed, while the iron-recovery ceiling is 81.6%, with a realistic band of approximately 76–81%; these ceilings assume complete conversion of hematite and siderite without over-reduction, full use of the internal reductants (pyrite-derived S2 and siderite-derived CO), and magnetic separation at the benchmark efficiency (0.12 T). The first roasting stage removes at most 42.9% of the sulfur; the remainder stays in magnetic pyrrhotite, and at least 95.6% of it must be removed in a second stage to bring the concentrate below 0.10% S. The results provide operating boundaries and performance expectations for subsequent engineering realization.

Keywords

Iron ore tailings; Pyrite; Magnetization roasting; Microwave heating; Desulfurization; Thermodynamic modelling