Fatigue behavior of geopolymer concrete (GPC) is important for pavement and structural systems subjected to repeated loading. This study investigates the fatigue performance of modified geopolymer concrete by examining the effects of activator molarity and material modifications using fly ash (FA), alccofine (AF), nano-silica (NS), I-Crete, and banana fiber (BF). Six geopolymer concrete mixtures were developed using 90% FA and 10% AF. The control mixtures were prepared with 8, 10, and 12 M NaOH and sodium silicate (Na₂SiO₃), while the modified mixtures incorporated 2% nano-silica, 2% I-Crete, and 2% banana fiber at 12 M NaOH. Fatigue loading tests were conducted on beam specimens (100 mm × 100 mm × 500 mm) at a frequency of 2 Hz and stress levels of 0.8 and 0.9. Fatigue behavior was evaluated using two-parameter Weibull analysis and reliability-based design fatigue-life assessment. The Weibull parameters increased with increasing activator molarity and material modification, particularly at a stress level of 0.8. Material modifications improved fatigue resistance, with banana-fiber-modified geopolymer concrete exhibiting the highest fatigue performance. At a failure probability of 0.01, the design fatigue life ranged from 2,184 to 4,831 cycles, while at a failure probability of 0.05, it ranged from 3,147 to 6,335 cycles. The endurance limit after 2 million loading cycles remained relatively stable, ranging from 49.0% to 50.5% of the flexural strength. Overall, increasing activator molarity and incorporating material modifications enhanced the fatigue resistance of geopolymer concrete, with banana fiber providing the most pronounced improvement.